6

Kubvisa Mhangura kubva kuCopper Smelter Slag ine Pyrite kana Flotation Tailings Inoteverwa neMvura Leaching

Tekinoroji Chikwata kubva kuUrbanMines chakasimbisa chidzidzo chekuchera mhangura kubva kune inonyungudutsa slag, iyo inoiswa pasi sulphating. Sulphating ye slag yakaitwa napyriteconcentrate kana flotation tailings patembiricha kubva 500 kusvika 650°C, uye calcine yakakonzerwa yakanyungudutswa nemvura.Zvigumisiro zvakaratidza kuti mhangura yakawanda yemhangura (70-73%) inowanikwa kubva kune calcine, inowanikwa nemaawa maviri neawa matatu sulphating pa 550 o C. Nzira yacho inosarudza sezvo 3-5% chete yesimbi inonyungudutswa.Mukuwedzera kune tembiricha ye sulphating, zvakaonekwa kuti mhedzisiro yakakura pamhangura leaching ine pyrite/flotation tailings: ratio.Migumisiro yakanakisisa yakawanikwa ne sulphating ye 5.00 g slag ne 2.00 g yepyrite kana 3.00 g yemaswe.

Pyrite MinePyrite OrePyrite Zvigadzirwa

Kunyungudutsa Mhangura kuburikidza neAdditive

Furidzira mweya uye kupisa kuti uite iron uyepyritekusvika padanho re oxidation

2CuFeS2 + 3O22CuS + 2FeO + 2SO2

 

 

Pisa calciate, quartz uye pyrite kusvika 1100

 

CuS + S(mu pyrite+ O2Cu2S + SO2

 

Zvichakadaro sezvo cupric sulfide inonaya

 

CaCO3 + SiO2CaSiO3 + CO2

 

CaSiO3 + FeO + SiO22(Fe,Ca)SiO3

 

Saka gadzira iron oxide yakasanganiswa nechitofu dregs uye uzviparadzanise

 

 

Bvisai cupric sulfide uye kufemera mumhepo

 

Cu2S + O22Cu + SO2

 

 

Kana zvichidiwa, ita mamwe magetsiolytkusanganisa ne sulfuric acid uye cupric sulfide solution

 

 

Gadzirisazve goridhe, sirivha uye platinamu kubva kune yakanaya isina kuchena

 

 

Chengetedza mutobvu wakabviswa musimbi panzvimbo iri pamusoro peinonyungudika

 

Mhangura ine nzvimbo yakakwira yekunyungudika inopatsanura yoyangarara ichikwira